Products
Home / Products / PU Waterproof Coating /

No Organic Solvent Water Based PU Waterproof Coating For Enclosed Space

No Organic Solvent Water Based PU Waterproof Coating For Enclosed Space

Brand Name: shhous
Model Number: Water‑borne eco‑friendly polyurethane coating
MOQ: 1000kg
Price: USD 0.8‑1.0/kg
Supply Ability: 1000000kg per Month
Detail Information
Place of Origin:
Shandong, China
Certification:
ISO
Solid Content /%:
≥65
Surface Dry:
≤4
Through Dry:
≤8
Elongation At Break /%:
≥300
Low-temperature Flexibility:
No Crack At -10℃
Waterproofness (0.3MPa, 30min):
No Water Penetration
Substrate Requirement:
Dry Solid Substrate Preferred; Cures By Air Moisture, Standing‑water Surface Forbidden
Application Method:
Cold‑applied By Troweling Or Brushing
Packaging Details:
Pails+Bags
Highlight:

water based pu waterproof coating

,

no organic pu waterproof coating

,

no organic polyurethane waterproofing coating

Product Description

No Organic Solvent Water-based Polyurethane Waterproof Coating For Enclosed Space

Water‑based Polyurethane Waterproof Coating Construction Procedure

  1. Substrate Preparation Make substrate solid and flat. Remove dust, oil and loose mortar. Repair cracks and holes with repair mortar. Damp substrate is acceptable, standing‑water is forbidden.
  2. Detail Reinforcement Apply 1‑2 coats of coating as extra reinforcement layer for corners, pipe roots, floor drains and construction joints. The width of extra layer ≥250 mm on each side. Proceed to main‑area construction after drying.
  3. Material Stirring One‑component product. Stir thoroughly after opening bucket. Do not dilute with water arbitrarily. Seal bucket lid during construction break to prevent skin formation caused by water evaporation.
  4. Multi‑layer Application Apply by brush, roller or trowel. Apply thin coats repeatedly; heavy single‑coat is prohibited. Apply next coat after previous coat dries, paint in cross directions to reach designed film thickness. Drying speed slows down under high‑humidity and low‑temperature, extend interval time properly.
  5. Curing & Drying Natural curing and drying. Protect coating from rain, ponding, treading and sharp‑object damage during curing.
  6. Inspection & Water‑storage Test Check for missing coating, pinholes, bubbles and other defects after full drying. Carry out 24‑48‑hour water‑storage test for water‑holding areas to ensure no leakage.
  7. Protective Layer Construction Construct cement‑mortar protective layer after acceptance. It has average UV resistance. Protective covering is required for exposed areas, direct exposure is not recommended.
No. Test Item Technical Index
Type Ⅰ Type Ⅱ
1 Solid Content /% ≥   65 65
2 Drying Time Surface Dry ≤ 4 4
Through Dry ≤ 8 8
3 Tensile Strength /MPa 1 1.5
4 Tensile Strength Retention after Treatment /% Heat Treatment ≥ 80 80
Alkali Treatment ≥ 60 60
Acid Treatment ≥ 40 40
Artificial Weathering ≥ 80-150
5 Elongation at Break /% ≥ 300 300
6 Elongation at Break after Treatment /% Heat Treatment ≥ 200 200
Alkali Treatment ≥ 200 200
Acid Treatment ≥ 200 200
Artificial Weathering ≥ 200
7 Low-temperature Flexibility (∅10mm mandrel) No crack at -10℃ No crack at -20℃
8 Waterproofness (0.3MPa, 30min) No water penetration No water penetration
9 Thermal Expansion/Contraction Rate /% Elongation ≤ 1 1
Contraction ≤ 1 1

No Organic Solvent Water Based PU Waterproof Coating For Enclosed Space